Ranking Materials for Extreme Sour Gas Service Using the Slow Strain Rate Method /

Equipment for use in sour gas wells is exposed to high-chloride brines saturated with hydrogen sulfide (H2S) and carbon dioxide (CO2) at temperatures up to 260°C (500°F). Both hydrogen-induced cracking and stress corrosion cracking are possible. However, traditional methods for testing environmental...